Large Quartz Glass Ring Cutting: 420 mm OD, Edge Chipping Under 0.2 mm
A fused quartz glass ring. 420 mm outer diameter, 300 mm inner bore, 18 mm thick. The ring has to come out intact — one piece, no cracks, edges clean
CUSTOMER STORIES
Real cutting tests, application examples, and customer-side material results from Vimfun endless diamond wire saw systems.

A fused quartz glass ring. 420 mm outer diameter, 300 mm inner bore, 18 mm thick. The ring has to come out intact — one piece, no cracks, edges clean

Diamond wire cutting high value brittle materials requires a fundamentally different approach from cutting structural metals or standard optical glass. When you are cutting a block of germanium worth several

A 300 mm diameter alumina ceramic ring. High purity. A cutting trial for a customer in Germany. At this scale, the challenge is not just holding a tolerance — it’s

Pure tungsten cracks at room temperature. Not sometimes — almost always, if your cutting method generates any lateral force. We had a customer ship us a 25 mm diameter tungsten

Titanium fights back when you cut it. We learned this the hard way — a customer sent us Ti-6Al-4V turbine blade blanks for sample sectioning. The first cut looked perfect.

SmCo magnets crack without warning. We’ve had a customer send us a batch of Sm2Co17 arc segments — 40 pieces total — and ask why their blade saw was destroying

NdFeB magnets are strong, compact, and easy to damage during cutting. The problem is not only hardness. In NdFeB magnet cutting, the real trouble usually comes from brittle grain fracture,

Hard metal cutting is where most conventional tools fail fast. Titanium alloys, tungsten, and molybdenum share a reputation that anyone who’s machined them knows well: they destroy tooling. Ti-6Al-4V eats

Buying a magnet cutting machine is a decision most shops only make once every 5–10 years. Get it right, and the machine pays for itself in reduced scrap, better surface
Something went wrong with your cut. The edges are chipped, the surface is grey, the thickness varies across the slice, or the wire broke mid-cut and now you’ve got a
Don’t worry! We know that obtaining cutting machines that meet your needs can be very challenging. Our professional cutting experts are always available to support you: